Products
  • Products
  • Categories
  • Blog
  • Podcast
  • Application
  • Document
|
GET A QUOTE
/ en
Select Language
Stanford Advanced Materials English
Stanford Advanced Materials Española
Stanford Advanced Materials Deutsch
Stanford Advanced Materials Français
Stanford Advanced Materials Italiano
Stanford Advanced Materials
/ en
Select Language
Stanford Advanced Materials English
Stanford Advanced Materials Española
Stanford Advanced Materials Deutsch
Stanford Advanced Materials Français
Stanford Advanced Materials Italiano

NI5369 K465 Nickel-based Superalloy Spherical Powder

Catalog No. NI5369
Grade K465
Shape Spherical Powder
Density 8.1-8.3g/cm3
Particle Size 10 to 75μm

K465 Nickel-based Superalloy Spherical Powder is an advanced nickel-based superalloy renowned for its exceptional combination of high strength and corrosion resistance, particularly in elevated temperature environments. Stanford Advanced Materials (SAM) boasts extensive experience in providing Nickel-based Alloy Spherical Powder with both high purity and competitive pricing.

Related products: Spherical Inconel 718 (UNS N07718) Powder (3D Printing Material), Spherical Inconel 939 Powder, Nickel Chromium Aluminum Yttrium Powder (NiCrAlY)

INQUIRY
Add to Inquiry List
K465 Nickel-based Superalloy Spherical Powder
K465 Nickel-based Superalloy Spherical Powder
K465 Nickel-based Superalloy Spherical Powder
K465 Nickel-based Superalloy Spherical Powder
K465 Nickel-based Superalloy Spherical Powder
K465 Nickel-based Superalloy Spherical Powder
Description
Specification
Technical Data Sheet

K465 Nickel-based Superalloy Spherical Powder Description

K465 Nickel-based Superalloy Spherical Powder is an advanced nickel-based superalloy renowned for its exceptional combination of high strength and corrosion resistance, particularly in elevated temperature environments. Tailored for aerospace, power generation, and chemical processing industries, K465 has emerged as a preferred choice where components face the challenges of extreme temperatures and aggressive conditions. This alloy not only withstands the rigors of these demanding sectors but also facilitates the creation of intricate 3D-printed geometries, optimizing overall performance. It meets the stringent requirements of aerospace, power generation, and chemical processing, ensuring reliability and longevity in the face of challenging operational conditions.

K465 Nickel-based Superalloy Spherical Powder Specifications

Density

8.1-8.3 g/cm3

Melting Point

1260-1350℃

Thermal Conductivity

11-16 W/m·K

Tensile Strength

1050-1250 MPa

Yield Strength

750-950 MPa

Elongation

10-25%

Hardness

35-45 HRC

K465 Nickel-based Superalloy Spherical Powder Applications

  • Aerospace: high strength and corrosion resistance at elevated temperatures, making it a vital choice for aircraft and spacecraft components.
  • Power Generation: From turbine components to critical elements in power plants, K465 ensures reliability and longevity, contributing to the efficiency and stability of power generation processes.
  • Automotive: This advanced nickel-based superalloy offers a winning combination of high strength and corrosion resistance, addressing the demanding conditions within automotive applications.
  • Chemical Processing: This nickel-based superalloy delivers robust strength and corrosion resistance, making it an ideal choice for critical components in chemical processing plants.

K465 Nickel-based Superalloy Spherical Powder Packaging

Our K465 Nickel-based Superalloy Spherical Powder is carefully handled during storage and transportation to preserve the quality of our product in its original condition.

GET A QUOTE

Send us an Inquiry now to find out more Information and the latest prices,thanks!

* Your Name
* Your Email
* Product name
* Your Phone
* Country

United States

    Shape

    Spherical

    • Spherical
    • Angular
    • Other
    Size

    15-53um

    • 15-53um
    • 45-150um
    • Other
    Quantity (Please specify in kg)
    Comments
    * Check Code
    Leave A Message
    Leave A Message
    * Your Name:
    * Your Email:
    * Product name:
    * Your Phone:
    * Comments: