Catalog No. | LM4519 |
BET | 7.1 m2/g |
Tap Density | 2.15 g/cm3 |
Bulk Density | 1.55 g/cm3 |
PH | 6.55 |
Moisture | 0.6 wt% |
NCM523 Cathode Precursor (Nickel-Cobalt-Manganese) is prepared by the co-precipitation method after adjusting the molar ratio of transition metal ions. Stanford Advanced Materials (SAM) has rich experience in manufacturing and supplying high-quality NCM523 Cathode Precursor (Nickel-Cobalt-Manganese).